Author: Subject: Powder coating tempretures
scutter

posted on 14/5/06 at 04:37 PM Reply With Quote
Powder coating tempretures

OK after a winter of driving the front ball joints and trackrod ends are looking shody,

The question is will the said joints withstand the temps involved with powdercoating?

ATB Dan.

View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
pathfinder

posted on 14/5/06 at 04:54 PM Reply With Quote
I doubt it very much! There is only one way to find out though
View User's Profile View All Posts By User U2U Member
paulf

posted on 14/5/06 at 08:09 PM Reply With Quote
They would need to be shotblasted first which would not do them any good and then heated to about 180c so I think not.
Paul.

View User's Profile View All Posts By User U2U Member
paulf

posted on 14/5/06 at 08:11 PM Reply With Quote
They would need to be shotblasted first which would not do them any good and then heated to about 180c so I think not.
Paul.

View User's Profile View All Posts By User U2U Member
scutter

posted on 15/5/06 at 06:26 AM Reply With Quote
Bugger, looks like some Smoothrite.

Thanks Dan.

View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member

New Topic New Poll New Reply


go to top






Website design and SEO by Studio Montage

All content © 2001-16 LocostBuilders. Reproduction prohibited
Opinions expressed in public posts are those of the author and do not necessarily represent
the views of other users or any member of the LocostBuilders team.
Running XMB 1.8 Partagium [© 2002 XMB Group] on Apache under CentOS Linux
Founded, built and operated by ChrisW.