Author: Subject: Cold (resin) casting
turbodisplay

posted on 8/5/08 at 06:08 PM Reply With Quote
Cold (resin) casting

Hi,
I`m making a dash board and the case mould has been made up of 10mm ali laser cut, then arranged to build up a 3d mould using 12mm bolts.

I have made up a case using normal resin (polyester?).
I left it for 3-4 hours before removing from the mould. The problem i have is the case is concave by 3mm on the long thin sections of the case.

I`m going to get a mould made up from the case to allow many to be produced, so i require a perfect case (buck
) to start with.
Would leaving it in the mould longer reduce the distortion?
I have thought about using polyurathane or epoxy instead. Is there any resins designed to have no shrinkage?

Thanks
Darren

NOTE:This user is registered as a LocostBuilders trader and may offer commercial services to other users
View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
Triton

posted on 8/5/08 at 07:06 PM Reply With Quote
The longer it's left to cure in the mould the better the product will be as fibreglass is a weird old fruit and will move all over the place.

Mark





My Daughter has taken over production of the damn fine Triton race seats and her contact email is emmatrs@live.co.uk.

www.tritonraceseats.com

www.hairyhedgehog.com

View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
balidey

posted on 8/5/08 at 07:49 PM Reply With Quote
Is it pure resin you're using? When ever I've done casting work I've added a filler. Usually a chalk based very very fine powder, but other bulk fillers are available. The filler really helps reduce shrinkage, because no matter how long you leave pure resin it WILL contract.
View User's Profile View All Posts By User U2U Member
turbodisplay

posted on 8/5/08 at 08:08 PM Reply With Quote
Thanks for your replies.
Been using chopped strands, for one, tring pure resing for next as the last one one had air trapped on surface.
Goos idea re filler, if it were 20% resin then only that could shrink.
I`ll try talc tomorow as a filler.
Thanks
Darren

NOTE:This user is registered as a LocostBuilders trader and may offer commercial services to other users
View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
twybrow

posted on 8/5/08 at 09:04 PM Reply With Quote
Look for a polyester casting resin. General purpose GRP type polyester resin just shrinks too much.

It would help to use low catalyst levels (especially with the hot weather) and cure as slowly as possible. Whatever happens, it will shrink.






View User's Profile View All Posts By User U2U Member
Chippy

posted on 8/5/08 at 10:14 PM Reply With Quote
As has been said previously, you need to leave the item in the mould for three or four days, not hours, for it to fully cure. If you are making the master copy, and then intend to make a mould of that so you can cast a few/many, then you will need to leave the item for a couple of weeks, to allow all of the resin to harden completely, otherwise when you try to pull a mould from it both items will stick together, (regardless of using a release agent). If you want your buck to remain nice and flat, you can add some reinforcing on the reverse side, thin strips of wood, etc, and put your chopped strand, pre wetted out, over them. HTH Ray





To make a car go faster, just add lightness. Colin Chapman - OR - fit a bigger engine. Chippy

View User's Profile E-Mail User View All Posts By User U2U Member

New Topic New Poll New Reply


go to top






Website design and SEO by Studio Montage

All content © 2001-16 LocostBuilders. Reproduction prohibited
Opinions expressed in public posts are those of the author and do not necessarily represent
the views of other users or any member of the LocostBuilders team.
Running XMB 1.8 Partagium [© 2002 XMB Group] on Apache under CentOS Linux
Founded, built and operated by ChrisW.