Printable Version | Subscribe | Add to Favourites
New Topic New Poll New Reply
Author: Subject: Pre-colored aluminum
derf

posted on 4/8/04 at 12:30 PM Reply With Quote
Pre-colored aluminum

I stopped by my local metal supply store, actually circle track (dirt racers) to pick up some steel last night, and I saw that they had 4'x8' and 4' x10' aluminum sheets, in plain aluminum and every color under the sun, price wasnt bad either $32US about $18UK, for each sheet in color, After I got home I started to think about it, would it be possible to use the colored sheets, or would the finish crack, would I have problems trying to form it around the rear corners or can I just beat it with a hammer and be done with it. And finally does anyone else have experience with the colored aluminum?
View User's Profile View All Posts By User U2U Member
ned

posted on 4/8/04 at 12:48 PM Reply With Quote
How was it coloured? painted, anodised or some other process?

Both can scratch and not polish out as easily as plainali does.

not that i know everything about coloured ali of course!

Ned.





beware, I've got yellow skin

View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
white130d

posted on 4/8/04 at 12:50 PM Reply With Quote
Coating

Derf, was it painted or was it anodized. It it was painted, then you do run the risk of having it flake off, if it's anodized, then no worries.

David
spending my day paintin' aluminum Land Rovers....





"There's only 2 things that money can't buy, and that's true love and home grown tomatos" Guy Clark

View User's Profile Visit User's Homepage View All Posts By User U2U Member
tom_loughlin

posted on 4/8/04 at 05:34 PM Reply With Quote
anodising is the way to go - did it a few years ago when in school, and the finish is spot on!!and very durable too.
i dont know why more people dont use it to be honest.
is it just aluminium that u can anodise - its done by applying a solvent to kind of etch the surface isnt it, then dunking it in dye, and sealing??
is there any way steel could be done?
a se7en with anodised bodywork would look awesome!!!

View User's Profile E-Mail User View All Posts By User U2U Member
Chris_R

posted on 4/8/04 at 06:46 PM Reply With Quote
At work we use pre-painted ali panels. We get a local company to fold them and they don't flake. Suppose it may depend on the brand though.





A bit of slapstick never hurt anyone.

http://www.chris.renney.dsl.pipex.com/



View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
SeaBass

posted on 4/8/04 at 06:54 PM Reply With Quote
Anodising starts to fade after a while and how would you match this with GRP etc???

Cheers






View User's Profile View All Posts By User U2U Member
derf

posted on 4/8/04 at 07:08 PM Reply With Quote
I just called the guy and he wasnt sure how it was colored, he said they bake it on, which is one of the processes in anodizing, so I'll go out on a limb and say anodized. As far as matching it, I would get the glass painted to match the color.

Anyway, I would have them cut the pieces into the right sizes with their bench shear, and just fold it around, my only thought was the rear around the corners, that might be hard to get formed to the right shape, I'd be beating on it all day, but the guy said that they bend them and beat on them and such....

View User's Profile View All Posts By User U2U Member
mangogrooveworkshop

posted on 4/8/04 at 08:16 PM Reply With Quote
picked off the tasty nuts website about anodizing

ALUMINIUM TECHNICAL SPECIFICATION

MATERIAL SPECIFICATIONS: 7075T73 high tensile aluminium.
MANUFACTURING PROCESS:
Head - cold formed: shank - thread rolling.
ULTIMATE STRENGTH (PSI): Chemically brightened and colour anodised to between 8 and 12 microns thick.
YEILD STRENGTH (PSI): 490-560Mpa; stronger than mild steel.
WEIGHT: 60% lighter than steel; 40% lighter than titanium.
CORROSION: Anodised aluminium is not affected by saltwater, road film or mild acids.
APPLICATIONS: Aluminium is suitable for use in all non-safety critical areas e.g. mudguards, screens, fairings, engine casings, huggers, fuel caps, number plates, lamp units, exhaust cans, heel plates, clutch levers, exhaust manifold brackets, fuel cap surround, air filter plus many more.

SAFETY:
Do not use Aluminium in any safety critical areas.

View User's Profile View All Posts By User U2U Member
white130d

posted on 4/8/04 at 08:29 PM Reply With Quote
Not Safe

So I guess all these RV8s I have sitting around aren't safe....





"There's only 2 things that money can't buy, and that's true love and home grown tomatos" Guy Clark

View User's Profile Visit User's Homepage View All Posts By User U2U Member
Mark Allanson

posted on 4/8/04 at 08:48 PM Reply With Quote
quote:
Originally posted by white130d
So I guess all these RV8s I have sitting around aren't safe....



too damn right!! Have you ever driven a Deranged Rover





If you can keep you head, whilst all others around you are losing theirs, you are not fully aware of the situation

View User's Profile Visit User's Homepage View All Posts By User U2U Member
splitrivet

posted on 5/8/04 at 02:11 PM Reply With Quote
Anodising on ali scratches off with time as the control bars on my microlight will testify.
As for the strength side they build airplanes out of it dont they so I spose thats debateable,but like allan says when it corrodes it goes big style and if it starts corroding under the anodisation way hey have you got problems.
Cheers,
Bob





I used to be a Werewolf but I'm alright nowwoooooooooooooo

View User's Profile Visit User's Homepage View All Posts By User U2U Member

New Topic New Poll New Reply


go to top






Website design and SEO by Studio Montage

All content © 2001-16 LocostBuilders. Reproduction prohibited
Opinions expressed in public posts are those of the author and do not necessarily represent
the views of other users or any member of the LocostBuilders team.
Running XMB 1.8 Partagium [© 2002 XMB Group] on Apache under CentOS Linux
Founded, built and operated by ChrisW.