I've got an old horsebox, the main box is made of thick mahogony tongue and groove. How do you go about sealing it/making it weatherproof? I cleaned all the gaps nicely and put some clear silicon in which worked for about a week. Then the hot weather came and the tongue and groove contracted and ripped all the silicon away, leaving gaps again So silicon is out, i'd have to keep re-applying it year round. Is there any kind of super-duper 2pack/resin wood paint that can move with it? or is there another way? Hemp/rope + pine tar?






View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
mookaloid

posted on 6/6/09 at 07:47 AM Reply With Quote
Wrap it in aluminium sheet?





"That thing you're thinking - it wont be that."


View User's Profile E-Mail User View All Posts By User U2U Member
Benzine

posted on 6/6/09 at 07:49 AM Reply With Quote
quote:
Originally posted by mookaloid
Wrap it in aluminium sheet?


Too pretty to do that






View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
JoelP

posted on 6/6/09 at 08:37 AM Reply With Quote
id say that nothing solid could resist the movement and not crack. Maybe oil it? Will protect the wood at least, if not the contents






View User's Profile View All Posts By User U2U Member
trextr7monkey

posted on 6/6/09 at 09:05 AM Reply With Quote
Strip it bare then 3 good coats of Sadolin- stuff in the yellow tin, it breathes and moves with wood and shoulld last for donkeys years, no pun intended





http://www.flickr.com/photos/14016102@N00/ (cut and paste this dodgey link)

Our most recent pics are here:
http://s129.photobucket.com/albums/p211/trextr7monkey/

View User's Profile E-Mail User View All Posts By User U2U Member
ReMan

posted on 6/6/09 at 09:08 AM Reply With Quote
I would have thought oil too, varnish at a push
View User's Profile Visit User's Homepage View All Posts By User U2U Member
trextr7monkey

posted on 6/6/09 at 11:02 AM Reply With Quote
Teak oil etc Ok for iroko and teak where the natural oilyness of wood makes it difficult for other finishes to stick but if out side it needs applying every year. Mahogany will take a stain and isn't so durable so I'd stick with sadolin- as used on high quality doors and window frames etc which are subject to similar changes in weather as your hoss box.
Bit wet for those jobs today though





http://www.flickr.com/photos/14016102@N00/ (cut and paste this dodgey link)

Our most recent pics are here:
http://s129.photobucket.com/albums/p211/trextr7monkey/

View User's Profile E-Mail User View All Posts By User U2U Member
Chippy

posted on 6/6/09 at 11:15 PM Reply With Quote
You could do what the boating boys do with the teak deck joints, but not at all cheap. You need to clean out the joints with some form of scraper, back to fresh timber,there is some kind of primer that you should apply first, but cant remember what it's called, then gun in Sikaflex, (sp), and once that is dry clean of the excess. Not a quick fix, but done properly should last the life of the H/Box. HTH Ray





To make a car go faster, just add lightness. Colin Chapman - OR - fit a bigger engine. Chippy

View User's Profile E-Mail User View All Posts By User U2U Member
Benzine

posted on 7/6/09 at 09:49 AM Reply With Quote
quote:
Originally posted by Chippy
You could do what the boating boys do with the teak deck joints, but not at all cheap. You need to clean out the joints with some form of scraper, back to fresh timber,there is some kind of primer that you should apply first, but cant remember what it's called, then gun in Sikaflex, (sp), and once that is dry clean of the excess. Not a quick fix, but done properly should last the life of the H/Box. HTH Ray


That sounds pretty good, I think part of the problem with the silicon was that I wasn't cleaning the surfaces enough beforehand. What's sikaflex? I hear of it all the time, just another sealant like silicon? Any idea where I can find out what that primer is you mentioned?

Many thanks






View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
mr henderson

posted on 7/6/09 at 11:16 AM Reply With Quote
Are you trying to seal the wood, ie to stop it deteriorating in the weather, or ais the varying gaps int he t&g that are causing a problem?

If it's the former then I would go with the others who are suggesting oil or Sadolin, something that soaks into the surface rather than lies on it, like varnish.

If it's the latter then I would want to know more about the problem before making suggestions

John






View User's Profile View All Posts By User U2U Member
Benzine

posted on 7/6/09 at 01:25 PM Reply With Quote
quote:
Originally posted by mr henderson

If it's the latter then I would want to know more about the problem before making suggestions

John


It's the latter (the varying gaps) that's the problem. The wood itself, as old as it is, in in great condition (thanks to the rot resistant properties of mahogany)

What furhter information can I give about the problem? I'll try and explain a bit more but let me know what else I can add... In the winter the gaps are tiny (either no gap or roughly 1mm) With the recent hot weather the gaps have moved anything up to 4mm. In winter it leaked a little, now when the rain comes it can be pretty bad. The roof is fibreglass and I recently re-sealed that, so that's fine. It's the capillary action of water getting into the tongue and groove that's causing the problem. So I need a solution that takes the movement of wood into consideration






View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
mr henderson

posted on 7/6/09 at 02:16 PM Reply With Quote
Tongue and groove, unless it has really deep grooves and matching tongues (which is unlikely due to the material that would be lost during manufacture), isn't really suitable for creating a weatherproof structure as large as a horsebox. The expansion and contraction as the timber tries to establish moisture content equilibrium with the relative huidity is too great. T&G is ok for a panel the size of a door, but I presume we are talking about a much larger surface.

I studied this subject in depth many years ago when I was involved in guitar making, where it is vitally important to control moisture content.

I'll think about it some more, but at the moment I don't see an effectiveanswer to it.

John






View User's Profile View All Posts By User U2U Member
Benzine

posted on 7/6/09 at 02:39 PM Reply With Quote
Thanks for the info, John. I'm wondering whether it'd work if I put strips of wood on the T&G that attached to the upper section of wood, goes down over the T&G gap, but isn't attached to the lower tongue and groove, with a gap of a few mm so water can't go back up with capillary action. It'd mean you couldn't see the tongue and groove, but I could stain them to match the rest of the wood, and it would move with the wood when it expands/contracts...

That description may have made NO sense whatsoever ^

[Edited on 7/6/09 by Benzine]






View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
Chippy

posted on 7/6/09 at 10:07 PM Reply With Quote
Hi, in answer to your question, Sykaflex is a available from most marine chandlers, as is the primer. as I said its not a cheap option, but the flexability is quite huge, something like 100 percent flex, so 3mm gap sealed will remain watertight to 6mm, I have used it on boats, (very damp environment), and never had any problems with it.
Note to Mr Henderson, never knew they made guitars out of T & G, Cheers Ray





To make a car go faster, just add lightness. Colin Chapman - OR - fit a bigger engine. Chippy

View User's Profile E-Mail User View All Posts By User U2U Member
trextr7monkey

posted on 7/6/09 at 10:35 PM Reply With Quote
quote:
Originally posted by Benzine
if I put strips of wood on the T&G that attached to the upper section of wood, goes down over the T&G gap, but isn't attached to the lower tongue and groove, with a gap of a few mm so water can't go back up with capillary action. It'd mean you couldn't see the tongue and groove, but I could stain them to match the rest of the wood, and it would move with the wood when it expands/contracts...



Extending that line of thinking you could cover the whole mahogany set up with thin overlapping ship lap boards- cedar would be nice

You must be pretty attached to that horse taking all of this trouble......or is the horse some one elses toy which gets you garage time if it travels along in a snug dry box?

atb
Mike





http://www.flickr.com/photos/14016102@N00/ (cut and paste this dodgey link)

Our most recent pics are here:
http://s129.photobucket.com/albums/p211/trextr7monkey/

View User's Profile E-Mail User View All Posts By User U2U Member
Benzine

posted on 8/6/09 at 07:49 AM Reply With Quote
quote:
Originally posted by trextr7monkey

You must be pretty attached to that horse taking all of this trouble......or is the horse some one elses toy which gets you garage time if it travels along in a snug dry box?



Yeah, very attached. I'm in it at the mo on mobile internet And the horses have gone along with their rubber matts and division walls etc to be replaced by an equally hairy stallion :p












View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member

New Topic New Poll New Reply


go to top






Website design and SEO by Studio Montage

All content © 2001-16 LocostBuilders. Reproduction prohibited
Opinions expressed in public posts are those of the author and do not necessarily represent
the views of other users or any member of the LocostBuilders team.
Running XMB 1.8 Partagium [© 2002 XMB Group] on Apache under CentOS Linux
Founded, built and operated by ChrisW.